ASME SB-653 covers seamless and welded zirconium and zirconium alloy welding fittings, factory made from three grades of zirconium and zirconium alloys. The term welding fittings applies to butt-welding parts such as 45 and 90 degree elbows, 180 degree returns, caps, tees, reducers, lap-joint stub ends and other types. Hefei Tailan Metal supplies zirconium butt weld fittings to SB-653 for all three grades defined by the specification, dimensioned to ASME B16.9 and MSS SP-43 for mating with pipe ordered to ANSI B36.19.
| Grade | UNS | Description | Zr + Hf min, % | Tin, % | Nb, % |
|---|---|---|---|---|---|
| PZ 2 | R60702 | Unalloyed zirconium | 99.2 | – | – |
| PZ 4 | R60704 | Zirconium-tin | 97.5 | 1.0-2.0 | – |
| PZ 5 | R60705 | Zirconium-niobium | 95.5 | – | 2.0-3.0 |
Grades per SB-653 4.1. Composition limits per ASME SB-658 Table 1, which is the pipe specification that the fittings are used with and the source of the corresponding grade chemistry.
Each grade exists for a specific corrosion duty. R60702 is unalloyed zirconium and is the general answer to strong hydrochloric and sulphuric acid service and to seawater, where it has no alloying addition to complicate the corrosion behaviour. R60704 adds 1-2 % tin, which improves resistance to reducing acids and particularly to sulphuric acid. R60705 adds 2-3 % niobium, which raises strength and improves resistance to strong acid conditions at elevated temperature. The specification also ties grade to raw material: SB-653 Table 1 lists the permissible pipe, tube, plate, bar and forging stock for each grade, so the whole assembly can be ordered from one material family.
We supply SB-653 zirconium butt weld fittings as 45 and 90 degree elbows, 180 degree returns, caps, tees, concentric reducers, lap-joint stub ends and other types on enquiry. For fittings covered by ANSI B16.9 or MSS SP-43, or for fittings used with pipe ordered to ANSI B36.19, the sizes, shapes and dimensions are as specified in those standards. Confirm the specific nominal size, schedule and dimensional standard against our current stock before ordering.
Fittings are manufactured by forging, forming or shaping operations, which may include hammering, pressing, piercing, extruding, upsetting, rolling, bending, fusion welding, machining, or a combination of these, and the forming procedure is applied so that it will not produce injurious defects. Fittings containing welded seams or other joints made by welding are welded by welders, welding operators and welding procedures qualified under Section IX of the ASME Boiler and Pressure Vessel Code, and filler metal, where used, is the same grade as the base metal.
| Item | Requirement |
|---|---|
| Material specification | ASME SB-653 (seamless and welded zirconium and zirconium alloy welding fittings) |
| Grades | R60702 (PZ 2), R60704 (PZ 4), R60705 (PZ 5) |
| Dimensional standard | ASME B16.9, MSS SP-43, or ANSI B36.19 mating practice as applicable |
| Welding | Welded by welders, welding operators and procedures qualified to ASME Section IX; filler metal the same grade as the base metal |
| Stress relief | All welds on grade R60705 stress relief annealed within 14 days after welding to prevent delayed hydride cracking, per Supplementary Requirement S3 |
| Chemical composition | Per SB-653 7.1 and Table 1, from the grade raw material listed in SB-653 Table 1 |
| Tensile requirements | Per SB-653 8.1 and Table 1 |
| Hydrostatic test | All fittings capable of withstanding the test pressure prescribed in the applicable standards without failure, leakage or impairment of serviceability; hydrostatic tests performed when required by the purchase order (SB-653 10.1, 10.2) |
| Inspection | Manufacturer inspects material prior to shipment; purchaser may witness tests at the place of manufacture if specified on the purchase order (SB-653 11.1) |
| Property | R60702 | R60704 | R60705 |
|---|---|---|---|
| Zirconium + hafnium, min, % | 99.2 | 97.5 | 95.5 |
| Iron + chromium, % | 0.2 max | 0.2 to 0.4 | 0.2 max |
| Tin, % | – | 1.0 to 2.0 | – |
| Niobium, % | – | – | 2.0 to 3.0 |
| Hydrogen, max, % | 0.005 | 0.005 | 0.005 |
| Nitrogen, max, % | 0.025 | 0.025 | 0.025 |
| Carbon, max, % | 0.05 | 0.05 | 0.05 |
| Oxygen, max, % | 0.16 | 0.18 | 0.18 |
| Tensile strength, min, ksi [MPa] | 55 [380] | 60 [415] | 80 [550] |
| Yield strength, min, ksi [MPa] | 30 [205] | 35 [240] | 55 [380] |
| Elongation in 2 in. or 50 mm, min, % | 16 | 14 | 16 |
Chemical requirements per ASME SB-658 Table 1; mechanical requirements per ASME SB-658 Table 3. The strength difference between R60705 and the other two grades comes from the niobium addition and is the reason R60705 is preferred where pressure and temperature combine with corrosion.
Hydrochloric acid. Unalloyed zirconium R60702 is the established material for hydrochloric acid handling above roughly 70 °C where stainless steels fail, and it is used in reactors, agitator shafts, pump casings and the associated piping in chlor-alkali and organic synthesis plants.
Sulphuric acid. R60704 with its tin addition is selected for sulphuric acid, where the alloying addition improves resistance beyond what unalloyed zirconium achieves in reducing acid conditions.
Strong acid at elevated temperature. R60705 zirconium-niobium is used where corrosion and mechanical duty combine, and in high-pressure acid service, and it is also the grade to specify where strength matters because of the hydrogen embrittlement concern that drives the mandatory stress relief of welds.
Pharmaceutical and fine chemical. Zirconium fittings are used in the reactor and transfer piping of pharmaceutical intermediates where the process is aggressive and the material must not contaminate the product.
Seawater and water treatment. Unalloyed zirconium has a long record in seawater handling and in desalination, and is used where chloride pitting of stainless steels is a concern.
Zirconium is susceptible to hydrogen pickup and to delayed hydride cracking, so handling, storage and welding practice must control hydrogen and the welding consumables must be properly baked and managed. Our technical department can advise on the details for a specific assembly.
The manufacturer inspects the material covered by the specification prior to shipment. Chemical composition is verified per SB-653 7.1 and Table 1, and tensile properties per SB-653 8.1 and Table 1. Where the purchaser wishes to witness testing and inspection at the place of manufacture, this must be stated on the purchase order together with the tests to be witnessed; the manufacturer gives ample notice of the time and place of the designated tests, and if the purchaser representative does not attend, the requirement is treated as waived. Where required by the purchase order, hydrostatic tests are performed. For grade R60705, all welds are stress relief annealed within 14 days after welding to prevent delayed hydride cracking, in accordance with Supplementary Requirement S3.
Send us the grade (R60702, R60704 or R60705), the fitting type, the nominal size and schedule, the quantity, and the service conditions including acid type and concentration, temperature and pressure. We will confirm dimensional compliance to B16.9 or the applicable standard, the material route, the available delivery schedule and issue a quotation on request. State any requirement for stress relief heat treatment (Supplementary Requirement S3), hydrostatic testing, purchaser inspection or a specific certification format with the enquiry, and we will build it into the order rather than assume it.