ASME SB-514 covers nickel-iron-chromium alloys in the form of welded, cold-worked and annealed pipe for general corrosive service and heat-resisting applications. Three alloys are furnished: UNS N08800 (Incoloy 800), UNS N08810 (Incoloy 800H) and UNS N08120. Hefei Tailan Metal supplies SB-514 welded pipe in all three grades. It is the specification to specify when the service temperature exceeds the range of 800 and creep-rupture strength governs the design, which is exactly where the 800 family separates from the lower-temperature grades.
| Grade | UNS | Ni | Cr | Fe | Al | Ti | Nb | C |
|---|---|---|---|---|---|---|---|---|
| Incoloy 800 | N08800 | 30.0-35.0 | 19.0-23.0 | 39.5 min (A) | 0.15 min-0.60 max | 0.15 min-0.60 max | – | 0.10 max |
| Incoloy 800H | N08810 | 30.0-35.0 | 19.0-23.0 | 39.5 min (A) | 0.15 min-0.60 max | 0.15 min-0.60 max | – | 0.05 to 0.10 |
| Alloy 800 type | N08120 | 35.0 min-39.0 max | 23.0 min-27.0 max | Remainder | 0.40 max | 0.20 max | 0.4 min-0.9 max | 0.02 min-0.10 max |
(A) Iron shall be determined arithmetically by difference. Chemical requirements per ASME SB-514 Table 2.
Two distinctions carry the grade selection. First, aluminium and titanium are held as minimum-plus-maximum ranges for N08800 and N08810 rather than as maximums alone, because these elements form the gamma-prime strengthening phase that governs creep resistance above 1100 °F (593 °C). Second, N08120 replaces aluminium and titanium with niobium, so it is not a heat-treatment variant of 800 but a different alloy design with a different grain-structure target. The specification itself assigns N08800 to service temperatures up to and including 1100 °F (593 °C), and N08120 and N08810 to service above 1100 °F where resistance to creep and rupture is required.
We supply SB-514 welded pipe cut to length, with square-cut or bevelled ends to suit the buyer’s welding procedure, and in nominal sizes and wall thicknesses on enquiry. The nominal schedule table is published below; what that table does not tell you is what we hold in stock, because availability follows plate and sheet production. Confirm the specific size and wall against current stock before ordering.
Under SB-514 the pipe is made from flat-rolled alloy by an automatic welding process with no addition of filler metal. Subsequent to welding and prior to the final solution treatment, the material is cold worked either in both weld and base metal, or in the weld metal only. Pipe is furnished with a scale-free finish; where bright annealing is used, descaling is not necessary. Filler metal for downstream field welding is agreed with the purchaser and reported against the deposited weld metal analysis.
Every size below is the nominal dimension published in ANSI B36.19, reproduced from ASME SB-775 Table 1 — the general requirements specification for nickel and nickel-alloy welded pipe. SB-514 1.2 states that the specification covers the outside diameter and nominal wall shown in ANSI B36.19, and SB-514 3 requires material to conform to the current edition of B 775, so SB-775 Table 1 and Table 2 together set the sizes and the tolerances for every pipe we supply under this specification. The decimal thicknesses are nominal or average wall dimensions, which is how ASME defines them.
| NPS | OD (in) | OD (mm) | Sch 5S (in / mm) | Sch 10S (in / mm) | Sch 40S (in / mm) | Sch 80S (in / mm) |
|---|---|---|---|---|---|---|
| 1⁄8 | 0.405 | 10.29 | — | 0.049 / 1.24 | 0.068 / 1.73 | 0.095 / 2.41 |
| 1⁄4 | 0.54 | 13.72 | — | 0.065 / 1.65 | 0.088 / 2.24 | 0.119 / 3.02 |
| 3–8 | 0.675 | 17.15 | — | 0.065 / 1.65 | 0.091 / 2.31 | 0.126 / 3.2 |
| 1⁄2 | 0.84 | 21.34 | 0.065 / 1.65 | 0.083 / 2.11 | 0.109 / 2.77 | 0.147 / 3.73 |
| 3–4 | 1.05 | 26.67 | 0.065 / 1.65 | 0.083 / 2.11 | 0.113 / 2.87 | 0.154 / 3.91 |
| 1 | 1.315 | 33.4 | 0.065 / 1.65 | 0.109 / 2.77 | 0.133 / 3.38 | 0.179 / 4.55 |
| 11–4 | 1.66 | 42.16 | 0.065 / 1.65 | 0.109 / 2.77 | 0.14 / 3.56 | 0.191 / 4.85 |
| 11–2 | 1.9 | 48.26 | 0.065 / 1.65 | 0.109 / 2.77 | 0.145 / 3.68 | 0.2 / 5.08 |
| 2 | 2.375 | 60.33 | 0.065 / 1.65 | 0.109 / 2.77 | 0.154 / 3.91 | 0.218 / 5.54 |
| 21–2 | 2.875 | 73.03 | 0.083 / 2.11 | 0.12 / 3.05 | 0.203 / 5.16 | 0.276 / 7.01 |
| 3 | 3.5 | 88.9 | 0.083 / 2.11 | 0.12 / 3.05 | 0.216 / 5.49 | 0.3 / 7.62 |
| 31–2 | 4 | 101.6 | 0.083 / 2.11 | 0.12 / 3.05 | 0.226 / 5.74 | 0.318 / 8.08 |
| 4 | 4.5 | 114.3 | 0.083 / 2.11 | 0.12 / 3.05 | 0.237 / 6.02 | 0.337 / 8.56 |
| 5 | 5.563 | 141.3 | 0.109 / 2.77 | 0.134 / 3.4 | 0.258 / 6.55 | 0.375 / 9.52 |
| 6 | 6.625 | 168.28 | 0.109 / 2.77 | 0.134 / 3.4 | 0.28 / 7.11 | 0.432 / 10.97 |
| 8 | 8.625 | 219.08 | 0.109 / 2.77 | 0.148 / 3.76 | 0.322 / 8.18 | 0.5 / 12.7 |
| 10 | 10.75 | 273.05 | 0.134 / 3.4 | 0.165 / 4.19 | 0.365 / 9.27 | 0.5 / 12.7 |
| 12 | 12.75 | 323.85 | 0.156 / 3.96 | 0.18 / 4.57 | 0.375 / 9.52 | 0.5 / 12.7 |
| 14 | 14 | 355.6 | 0.156 / 3.96 | 0.188 / 4.78 | — | — |
| 16 | 16 | 406.4 | 0.165 / 4.19 | 0.188 / 4.78 | — | — |
| 18 | 18 | 457.2 | 0.165 / 4.19 | 0.188 / 4.78 | — | — |
| 20 | 20 | 508 | 0.188 / 4.78 | 0.218 / 5.54 | — | — |
| 22 | 22 | 558.8 | 0.188 / 4.78 | 0.218 / 5.54 | — | — |
| 24 | 24 | 609.6 | 0.218 / 5.54 | 0.25 / 6.35 | — | — |
| 30 | 30 | 762 | 0.25 / 6.35 | 0.312 / 7.92 | — | — |
Note A — Schedules 5S and 10S wall thicknesses do not permit threading in accordance with ANSI B1.20.1. Note B — These do not conform to ANSI B36.10.
Nominal size is not delivered size. The permissible variations in outside diameter for welded pipe are set out in ASME SB-775 Table 2 — they are the tolerances a mill is permitted to work to, and they are what you should hold the supplier to when the pipe arrives. State them on the purchase order so acceptance is objective rather than a conversation.
| NPS designator | Permissible variation in OD, over (in / mm) | Permissible variation in OD, under (in / mm) |
|---|---|---|
| 1⁄8 to 11⁄2, incl | 0.015 / 0.4 | 0.031 / 0.8 |
| Over 11⁄2 to 4, incl | 0.031 / 0.8 | 0.031 / 0.8 |
| Over 4 to 8, incl | 0.062 / 1.6 | 0.031 / 0.8 |
| Over 8 to 18, incl | 0.093 / 2.4 | 0.031 / 0.8 |
| Over 18 to 26, incl | 0.125 / 3.2 | 0.031 / 0.8 |
| Over 26 to 34, incl | 0.156 / 4 | 0.031 / 0.8 |
| Over 34 to 48, incl | 0.187 / 4.8 | 0.031 / 0.8 |
Note A — These permissible variations in outside diameter apply only to material as finished at the mill before subsequent swaging, expanding, bending, polishing, or other fabricating operations.
Note B — Ovality is the difference between the maximum and the minimum outside diameter measured at any one cross section. There is no additional tolerance for ovality on material having a nominal wall thickness for more than 3 % of the outside diameter. On this material, the average of the maximum and the minimum outside diameter measurements will fall within the outside diameter tolerance shown in the table. An additional ovality allowance of twice the outside diameter tolerance spreads shown in the table, applied ±½, is allowed for material having a nominal wall thickness of 3 % or less of the nominal outside diameter.
Note C — The wall thickness variation shall not exceed ±12.5 % of the nominal wall thickness.
For the size and tolerance cross-reference across the nickel alloy pipe and tube products we supply, see our nickel alloy round pipe and tube dimensional data. For the companion SB-705 welded nickel alloy pipe page, see our welded nickel alloy pipe under ASME SB-705.
| Item | Requirement |
|---|---|
| Material specification | ASME SB-514 (welded nickel-iron-chromium alloy pipe) |
| Alloys covered | UNS N08800, UNS N08810, UNS N08120 |
| Service range | N08800 up to and including 1100 °F (593 °C); N08120 and N08810 above 1100 °F for creep and rupture resistance |
| Annealing temperature | N08120 annealed at 2150 °F (1177 °C) minimum; N08810 annealed at 2050 °F (1120 °C) minimum (SB-514 8.4) |
| Grain size | Transverse sample representing full wall thickness of annealed N08120 and N08810 shall conform to an average grain size of ASTM No. 5 or coarser (SB-514 8.2) |
| Flattening test | Capable of withstanding flattening without cracking until the distance between platens is five times the wall thickness, weld positioned 90 degrees from the applied force |
| Nondestructive test | Category 1: each piece of each lot subjected to one of hydrostatic, pneumatic (air underwater), eddy current or ultrasonic; Category 2: each piece subjected to a leak test and an electric test |
| Certification | State on the purchase order if certification or a report of test results is required |
| Alloy | Condition | Tensile min, psi (MPa) | Yield 0.2 % min, psi (MPa) | Elongation in 2 in. or 50 mm, min, % |
|---|---|---|---|---|
| UNS N08120 | Annealed | 90 000 (621) | 40 000 (276) | 30 |
| UNS N08800 | Annealed | 75 000 (520) | 30 000 (207) | 30 |
| UNS N08810 | Annealed | 65 000 (450) | 25 000 (170) | 30 |
SB-514 Table 1. The lower strength of N08810 relative to N08800 is a direct consequence of the controlled grain size target, which is why the creep-resistant grades are specified on rupture data rather than on tensile numbers alone.
Steam and superheater systems. Welded 800H pipe is a standard selection for superheater and reheater tubing and headers in steam boilers, and for the crossover piping of thermal power plant, where the operating temperature sits above the range of the ferritic and austenitic stainless grades.
High-temperature process piping. Furnace and reformer piping, radiant coils and transfer lines in petrochemical and ammonia plants use N08120 where creep-rupture data governs the wall thickness calculation.
Thermal expansion and furnace internals. Welded 800 and 800H pipe is used in heat treatment furnace retorts, radiant tube supports and quench systems where thermal cycling and oxidation resistance both matter.
General corrosive service. The chromium level of the 800 family gives solid resistance to oxidising media, and the nickel content gives good behaviour in reducing conditions, so welded 800 pipe is also specified for caustic and acid-handling duties below 1100 °F (593 °C).
SB-514 sets the chemistry and the mechanical properties for the three alloys in this specification and sends every other requirement to ASME SB-775, the general requirements specification for nickel and nickel-alloy welded pipe; SB-514 4.1 requires material to conform to the applicable requirements of the current edition of B 775. The hydrostatic test rule is in that general requirements volume, and for welded pipe it is not the rule that governs seamless pipe.
SB-775 5.3.1 requires each length of pipe to be tested by the manufacturer to a minimum internal hydrostatic pressure of 1000 psi (6.9 MPa), provided the fibre stress calculated from P = 2St/D does not exceed the allowable fibre stress for the material. S is the lower of two thirds of the specified minimum 0.2 % offset yield strength or one quarter of the specified minimum ultimate strength, taken from the mechanical property table of the product specification. t is the minimum wall thickness permitted including the minus tolerance, and D is the nominal outside diameter.
Four provisions of this volume change the answer a buyer gets.
The wall thickness used in the equation comes from a different rule than the seamless case, and this is the step most often copied from the wrong table. For welded pipe the minus tolerance is the single flat value in ASME SB-775 Table 2, Note C: the wall thickness variation shall not exceed plus or minus 12.5 % of the nominal wall thickness, at every size. The minimum wall column below is the nominal wall reduced by that 12.5 %, so the pipe delivered at the low side of the tolerance band governs the test. ASME SB-829 Table 2 applies size-banded specified minimum wall percentages of 10.0, 12.5 and 15.0 % to seamless cold-worked pipe, and those bands are not correct for a welded order. For this, see our copper nickel seamless pipe dimensional data.
SB-514 publishes no allowable fibre stress table of its own, so the SB-775 5.3.1 formula is applied to the specified minimum strengths in SB-514 Table 1. For all three grades the governing term is the tensile strength: two thirds of the yield strength is the higher of the two in every case.
| Grade | Condition | Tensile strength min (psi) | Yield strength 0.2 % offset min (psi) | Allowable Fibre stress S (psi) | Source |
|---|---|---|---|---|---|
| UNS N08120 | annealed | 90,000 | 40,000 | 22,500 | ASME SB-514 Table 1 |
| UNS N08800 (Alloy 800) | annealed | 75,000 | 30,000 | 18,750 | ASME SB-514 Table 1 |
| UNS N08810 (Alloy 800H) | annealed | 65,000 | 25,000 | 16,250 | ASME SB-514 Table 1 |
Calculated for UNS N08800 in the annealed condition from the allowable fibre stress above, applying P = 2St/D with t as the minimum wall permitted, that is the nominal wall reduced by the ASME SB-775 Table 2 Note C minus tolerance of 12.5 %, and D the nominal outside diameter from the ASME SB-775 Table 1 dimensions published above. The other two grades scale directly from the same equation using their own allowable fibre stress; at NPS 4 Sch 40S the maximum test pressure is 1 728 psi for N08800, 1 498 psi for N08810 and 2 074 psi for N08120.
| NPS | Schedule | OD (in) | Nominal wall (in) | Minimum wall (in) | Allowable Fibre stress S (psi) | Maximum test pressure 2St/D (psi) | (MPa) | ASME 1000 psi achievable |
|---|---|---|---|---|---|---|---|---|
| 1/2 | Sch 40S | 0.840 | 0.109 | 0.0954 | 18,750 | 4,258 | 29.4 | Yes |
| 1 | Sch 40S | 1.315 | 0.133 | 0.1164 | 18,750 | 3,319 | 22.9 | Yes |
| 2 | Sch 40S | 2.375 | 0.154 | 0.1348 | 18,750 | 2,128 | 14.7 | Yes |
| 4 | Sch 40S | 4.500 | 0.237 | 0.2074 | 18,750 | 1,728 | 11.9 | Yes |
| 6 | Sch 40S | 6.625 | 0.280 | 0.2450 | 18,750 | 1,387 | 9.6 | Yes |
| 8 | Sch 40S | 8.625 | 0.322 | 0.2818 | 18,750 | 1,225 | 8.4 | Yes |
| 12 | Sch 10S | 12.750 | 0.180 | 0.1575 | 18,750 | 463 | 3.2 | No |
The last row is the case worth noting. At NPS 12 in Schedule 10S the maximum hydrostatic test pressure for UNS N08800 falls to 463 psi, below the ASME 1000 psi minimum, so a pipe in that size and schedule cannot be hydrostatically tested to the code minimum without exceeding the allowable fibre stress and has to be electrically examined under the Category 1 provisions instead. That is a manufacturing and commercial decision to settle at the enquiry stage, not a defect found at inspection.
Chemical analysis is performed to SB-514 Table 2 with the iron content determined arithmetically by difference, and a product (check) analysis by the purchaser is subject to the permissible variations in Table 1 of Specification B775. Tensile properties are verified per SB-514 Table 1. For annealed N08120 and N08810 the grain size requirement of ASTM No. 5 or coarser is verified on a transverse sample representing the full wall thickness. Every piece of every lot receives the nondestructive examination required by the category selected, and the category is stated on the purchase order. Certification and the report of test results are stated as required on the purchase order and form part of the shipment documentation.
Send us the grade (N08800, N08810 or N08120), the nominal size or outside diameter and wall thickness, the length, the quantity, and the service conditions including design temperature, design pressure and whether the service is oxidising or reducing. We will confirm dimensional compliance, the annealing route, the available delivery schedule and issue a quotation on request. If the order requires a specific nondestructive test category, a grain size verification, a witnessed inspection or a particular certification format, state it with the enquiry so it is included in the order.
Compare the current supplier pages for this alloy, each with dimensions, certification and RFQ information: