Copper-nickel 90-10 UNS C70600 and 70-30 C71500 seamless pipe and tube to ASME SB-466, welded pipe to SB-467. Seawater, firewater and heat exchanger use.
When a seawater intake screen, a firewater ring main or a ship’s ballast line has to survive chlorinated seawater for thirty years without replacement, the material question is usually settled with copper-nickel rather than nickel-chromium. The 90-10 and 70-30 copper-nickel alloys occupy a position that neither stainless nor nickel alloys fully occupy: they carry an inherently low corrosion rate in seawater, they do not suffer chloride stress-corrosion cracking, and they are dramatically cheaper per tonne than nickel-base material. This page covers the seamless tube to ASME SB-466 and the welded pipe to ASME SB-467, with 90-10 (UNS C70600, C70620) and 70-30 (UNS C71500, C71520) covered, together with the 95-5 and 80-20 variants where the application calls for them.
Each step up in nickel content buys a specific property: 90-10 is the general seawater workhorse, 70-30 adds strength and comes with a different corrosion behaviour in aerated seawater, and the intermediate grades fill narrower needs. The ASME SB-466 Table 1 chemical requirements and the matching SB-467 Table 1 give the following composition limits.
| Element | C70600 / C70620 (90-10) | C71500 / C71520 (70-30) | C72200 (80-20) | C70400 (95-5) |
|---|---|---|---|---|
| Copper (incl. silver), % | remainder / 86.5 min | remainder / 65.0 min | remainder | remainder |
| Nickel (incl. cobalt), % | 9.0–11.0 | 29.0–33.0 | 15.0–18.0 | 4.8–6.2 |
| Lead, max % | 0.05 / 0.02 | 0.05 / 0.02 | 0.05 | 0.05 |
| Iron, % | 1.0–1.8 | 0.40–1.0 | 0.50–1.0 | 1.3–1.7 |
| Zinc, max % | 1.0 / 0.50 | 1.0 / 0.50 | 1.0 | 1.0 |
| Manganese, max % | 1.0 | 1.0 | 1.0 | 0.30–0.8 |
| Chromium, % | not required | not required | 0.30–0.7 | not required |
| Carbon, max % | 0.05 (C70620) | 0.05 (C71520) | 0.05 | not required |
Note that C70620 and C71520 are the welding-modified grades. Their lead, zinc and carbon limits are tightened specifically so the alloys can be joined without hot cracking, and SB-467 Table 1 calls them out as separate entries for exactly that reason. If your fabrication involves welding, specify the modified grade.

SB-466 covers seamless copper-nickel pipe and tube for seven UNS designations, with outside-diameter and wall tolerances in Tables 3 to 6 and full heat-treatment condition designations. SB-467 covers the welded equivalent, with the as-welded, cold-drawn and fully-finished-and-annealed condition codes defined in the specification.
The mechanical property requirements differ meaningfully between 90-10 and 70-30 in the annealed condition, and SB-466 Table 2 sets them out by temper and alloy. For the fitting families used on the same systems, our nickel alloy butt weld fittings range covers the general butt-weld dimensional families, while our nickel alloy pipe and tube category lists every pipe and tube grade we hold.

From SB-466 Table 2, in the O60 soft anneal temper:
| Alloy | Tensile strength, min | Yield strength, min | Rockwell hardness |
|---|---|---|---|
| C70600 and C70620 (90-10) | 38 ksi (260 MPa) | 13 ksi (90 MPa) | 45 max |
| C71000 (80-20) | 45 ksi (310 MPa) | 16 ksi (110 MPa) | 48 max |
| C71500 and C71520 (70-30) | 52 ksi (360 MPa) | 18 ksi (125 MPa) | 51 max |
| C72200 | 40 ksi (275 MPa) | 14 ksi (95 MPa) | 45 max |
For welded pipe annealed to the WO61 condition, SB-467 Table 2 gives 90-10 a tensile strength of 40 ksi (275 MPa) and a 0.5 percent extension yield of 15 ksi (105 MPa) up to 4-1/2 in. outside diameter, and 70-30 a tensile of 50 ksi (345 MPa) with a 20 ksi (140 MPa) yield in the same size range. Both alloys require an expansion test in the annealed condition, and product over 4 in. (100 mm) may alternatively be subjected to the flattening test of Practice B968/B968M.
Commercial weight is what the freight is settled on, so it is worth being
precise about which density was used to calculate it. For copper-nickel alloys
ASME publishes the design density in ASME SB-111 Table X1.1, and for UNS C70600 and C71500 and their welding-grade equivalents
that figure is 0.323 lb/in.³ (8.94 g/cm³). This is the same
value that appears in the standard published physical-property data for 90/10
and 70/30 copper-nickel, so it is the number to use for a shipment calculation
rather than a self-estimated or indicative density.
Theoretical weight per unit length is then calculated from the outside
diameter and the wall thickness of the size being ordered, using the standard
pipe mass equation:
M = C × (D − t) × t
where M is mass per unit length in kg/m, D is the specified outside diameter
in mm, t is the specified wall thickness in mm, and C is π × ρ
÷ 1000 with ρ = 8.94 g/cm³ for this alloy. Unlike carbon
steel, where a single 7.85 g/cm³ factor applies, a copper-nickel order has
to be calculated at its own published density. As a check on the method
itself: carbon steel at 7.85 g/cm³ for NPS 4 Sch 40 reproduces the widely
published 16.08 kg/m, which confirms the equation and its unit handling before
it is applied to a copper-nickel size.
SB-466 Table X1.1 gives the preferred sizes and wall thicknesses for this
specification, and the table below reproduces it. The dimension basis is the
standard pipe size outside diameter rather than a nominal bore, and the table
carries a set of Specials columns alongside the Regular and Extra Strong wall
thicknesses. Note that the SB-466 outside diameter for SPS 5 in. is 5.552 in.
(141 mm), which differs from the ANSI B36.19 value of 5.563 in. used for
steel and stainless pipe: the preferred-size table is specific to this
specification, and the difference is the reason a copper-nickel order should
always name SB-466 rather than referring loosely to a nickel alloy pipe
schedule.
The table below gives the theoretical weight of each preferred size at the
Regular and Extra Strong wall thicknesses, calculated at the ASME SB-111
design density of 8.94 g/cm³.
| SPS (in) | OD, in. (mm) | Regular wall, in. (mm) | Regular wall, kg/m (lb/ft) | Extra Strong wall, in. (mm) | Extra Strong wall, kg/m (lb/ft) |
|---|---|---|---|---|---|
| 1/8 | 0.405 (10.3) | 0.062 (1.57) | 0.38 (0.26) | 0.1 (2.54) | 0.55 (0.37) |
| 1/4 | 0.54 (13.7) | 0.082 (2.08) | 0.68 (0.46) | 0.123 (3.12) | 0.93 (0.62) |
| 3/8 | 0.675 (17.1) | 0.09 (2.29) | 0.95 (0.64) | 0.127 (3.23) | 1.26 (0.85) |
| 1/2 | 0.84 (21.3) | 0.107 (2.72) | 1.42 (0.95) | 0.149 (3.78) | 1.86 (1.25) |
| 3/4 | 1.05 (26.7) | 0.114 (2.9) | 1.94 (1.30) | 0.157 (3.99) | 2.54 (1.71) |
| 1 | 1.315 (33.4) | 0.126 (3.2) | 2.71 (1.82) | 0.182 (4.62) | 3.73 (2.51) |
| 1-1/4 | 1.66 (42.2) | 0.146 (3.71) | 4.01 (2.69) | 0.194 (4.93) | 5.16 (3.47) |
| 1-1/2 | 1.9 (48.3) | 0.15 (3.81) | 4.76 (3.20) | 0.203 (5.16) | 6.25 (4.20) |
| 2 | 2.375 (60.3) | 0.156 (3.96) | 6.27 (4.21) | 0.221 (5.61) | 8.62 (5.79) |
| 2-1/2 | 2.875 (73) | 0.187 (4.75) | 9.11 (6.12) | 0.28 (7.11) | 13.16 (8.84) |
| 3 | 3.5 (88.9) | 0.219 (5.56) | 13.01 (8.75) | 0.304 (7.72) | 17.60 (11.83) |
| 3-1/2 | 4 (102) | 0.25 (6.35) | 17.06 (11.46) | 0.321 (8.15) | 21.48 (14.44) |
| 4 | 4.5 (114) | 0.25 (6.35) | 19.20 (12.90) | 0.341 (8.66) | 25.62 (17.22) |
| 5 | 5.552 (141) | 0.25 (6.35) | 24.01 (16.14) | 0.375 (9.52) | 35.15 (23.62) |
| 6 | 6.625 (168) | 0.25 (6.35) | 28.83 (19.37) | 0.437 (11.1) | 48.91 (32.87) |
It is worth showing the size of that difference in numbers, because the copper-nickel weight charts circulating in this industry are computed at carbon-steel density. Take SPS 1/2 in. from the table above, outside diameter 21.3 mm with the Regular wall of 2.72 mm: at the ASME SB-111 design density of 8.94 g/cm³ that is 1.42 kg/m, while the same size and wall calculated at the carbon-steel density of 7.85 g/cm³ is 1.25 kg/m. The difference is 13.9 %. A widely copied copper-nickel weight chart gives 1.27 kg/m for the equivalent NPS 1/2 Sch 40S geometry, which is reproduced exactly by the carbon-steel density, not by the copper-nickel one. For a buyer settling freight on mill certificate weights, that is not a rounding difference: it is the difference between paying for the metal that was shipped and paying for the carbon steel equivalent of it.
Two further points on how to use these figures. The weights are theoretical The weights are theoretical and are
calculated from nominal dimensions; actual mill weights will sit slightly
above them, and the applicable acceptance band is set by the general
requirements specification rather than by this table. And because the density
is a copper-nickel value, these figures are not interchangeable with the
weights quoted for carbon steel of the same size: a copper-nickel pipe of a
given wall is heavier than the carbon steel pipe of the same nominal size and
schedule, and a freight calculation built on the carbon steel figure will
understate the shipment weight. If your order specifies minimum wall rather
than nominal wall, the mass has to be recalculated on the specified minimum
wall, which is the same distinction that runs through the general-requirements
specification for stainless and alloy steel pipe.
Send the specification, the UNS designation, the outside diameter and wall thickness, the length, the temper or condition, and the quantity. For welded pipe specify whether the condition is as-welded, cold-drawn, or fully finished annealed; for seamless tube specify the temper (O60, H55 or H80). If the material will be welded into a system, state that clearly so we can confirm the modified grade. We will return availability, lead time and the inspection document package.
Our industry news and project case collection includes worked examples of seawater systems where copper-nickel was specified over nickel-base material on cost grounds, and our nickel alloy fittings overview is a good reference if the system also carries nickel-base components.
The UNS designations used above are set out in the nickel alloy grade cross-reference reference.
Copper-nickel pipe is proof tested on its own basis, and the seamless and welded specifications do not use the same one. Both arrive at the same fiber stress but reach it by different routes, and the size thresholds at which the tests are available differ.
ASME SB-466, the seamless specification, applies an electromagnetic (eddy current) test to every tube up to and including 3.125 in. [80 mm] nominal outside diameter under clause 11.2.1. Clause 11.2.2 makes the hydrostatic test an alternate to that eddy current test for tubes above 1.25 in. [32 mm] in diameter: the tube shall stand, without showing evidence of leakage, an internal hydrostatic pressure sufficient to produce a fiber stress of 7000 psi [48 MPa], calculated as P = 2St/(D − 0.8t) for a thin hollow cylinder under tension, and the tube need not be subjected to a pressure gage reading over 1000 psi [7 MPa] unless specifically stipulated in the contract or purchase order. Clause 11.2.3 allows a pneumatic test at a minimum internal air pressure of 60 psig [415 kPa] for 5 s, and clause 11.2.2.2 gives the manufacturer the option of the hydrostatic or the pneumatic test for tubes under 0.50 in. [12 mm] outside diameter with wall under 0.060 in. [1.5 mm].
ASME SB-467, the welded specification, has a wider eddy current obligation: clause 11.2 subjects each pipe within the capabilities of the eddy-current tester to that test. Clause 11.3 makes the hydrostatic test an alternative for tubes above 2.000 in. [50.8 mm], again at a fiber stress of 7000 psi [48 MPa] with the same P = 2St/(D − 0.8t) equation, and the pipe need not be tested at a hydrostatic pressure over 1000 psig [7 MPa] unless so specified. Clause 11.3.2 sets the pneumatic test at 60 psig (400 kPa) minimum for 5 s.
The 7000 psi fiber stress is a fixed value in both specifications rather than a fraction of the material’s yield strength, so the pressure depends only on the wall and the diameter. The table below gives two numbers for each size. The first is the pressure that produces the 7000 psi fiber stress clause 11.2.2 demands, calculated from the printed equation. The second is the pressure the tube is actually tested to, because clause 11.2.2.1 says the tube “need not be subjected to a pressure gage reading over 1 000 psi [7 MPa]” unless the contract or purchase order specifically stipulates otherwise. The 1 000 psi figure limits the gage reading, not the pressure the equation calls for: at SPS 1/8 Extra Strong the calculation returns 4 308 psi while the gage stops at 1 000 psi. For the wider picture, see our six hydrostatic test rules compared side by side.
These pressures are our own calculation from the printed formula and the printed dimensions. They are not values printed in the specification.
The practical point for a buyer is that 7000 psi is a modest fraction of the strength of either alloy, so on the thinner walls the calculated pressure falls below 1 000 psi and the test is set by geometry alone, with no relief from the gage-reading clause. On the regular wall the calculated pressure is 1 155 psi at SPS 1/2, then 721 psi at SPS 1, 503 psi at SPS 2 and 288 psi at SPS 6. On the extra strong wall the calculated pressure stays above 1 000 psi from SPS 1/8 through SPS 4 (2 378 psi at SPS 3/4 and 1 129 psi at SPS 4), reaches 1 000 psi at SPS 5 and drops to 975 psi at SPS 6, so from SPS 5 onward the full calculated pressure applies. For 90-10 and 70-30 this is not a weak test. It is a corrosion-service tube test, and the 7000 psi figure is the same in both the seamless and welded specifications because it is a property of the alloy family rather than of the manufacturing route.
One structural difference between the two documents is worth noting for anyone assembling a specification. SB-466 clause 3.1 adopts the general requirements of ASTM B251/B251M for terminology, materials and manufacture, dimensions, mass and permissible variations, workmanship, finish and appearance. SB-467 has no such general requirements section and stands on its own, drawing only on the test methods and the American Welding Society filler metal specifications it names. A seamless copper-nickel order and a welded copper-nickel order are therefore not governed by a common framework, and inspection and certification obligations do not carry across from one to the other.
| SPS | Wall | Nominal wall, in. | OD, in. | Pressure for 7 000 psi fiber stress, psi | MPa | Pressure the tube is tested to, psi | Basis |
|---|---|---|---|---|---|---|---|
| 1/8 | Regular | 0.058 | 0.405 | 2,264 | 16 | 1,000 | Gage limited to 1 000 psi |
| 1/8 | Extra Strong | 0.100 | 0.405 | 4,308 | 30 | 1,000 | Gage limited to 1 000 psi |
| 1/4 | Regular | 0.065 | 0.540 | 1,865 | 13 | 1,000 | Gage limited to 1 000 psi |
| 1/4 | Extra Strong | 0.123 | 0.540 | 3,899 | 27 | 1,000 | Gage limited to 1 000 psi |
| 3/8 | Regular | 0.065 | 0.675 | 1,461 | 10 | 1,000 | Gage limited to 1 000 psi |
| 3/8 | Extra Strong | 0.127 | 0.675 | 3,101 | 21 | 1,000 | Gage limited to 1 000 psi |
| 1/2 | Regular | 0.065 | 0.840 | 1,155 | 8 | 1,000 | Gage limited to 1 000 psi |
| 1/2 | Extra Strong | 0.149 | 0.840 | 2,894 | 20 | 1,000 | Gage limited to 1 000 psi |
| 3/4 | Regular | 0.065 | 1.050 | 912 | 6 | 912 | Full calculated pressure |
| 3/4 | Extra Strong | 0.157 | 1.050 | 2,378 | 16 | 1,000 | Gage limited to 1 000 psi |
| 1 | Regular | 0.065 | 1.315 | 721 | 5 | 721 | Full calculated pressure |
| 1 | Extra Strong | 0.182 | 1.315 | 2,179 | 15 | 1,000 | Gage limited to 1 000 psi |
| 11/4 | Regular | 0.072 | 1.660 | 629 | 4 | 629 | Full calculated pressure |
| 11/4 | Extra Strong | 0.194 | 1.660 | 1,805 | 12 | 1,000 | Gage limited to 1 000 psi |
| 11/2 | Regular | 0.072 | 1.900 | 547 | 4 | 547 | Full calculated pressure |
| 11/2 | Extra Strong | 0.203 | 1.900 | 1,636 | 11 | 1,000 | Gage limited to 1 000 psi |
| 2 | Regular | 0.083 | 2.375 | 503 | 3 | 503 | Full calculated pressure |
| 2 | Extra Strong | 0.221 | 2.375 | 1,408 | 10 | 1,000 | Gage limited to 1 000 psi |
| 21/2 | Regular | 0.083 | 2.875 | 414 | 3 | 414 | Full calculated pressure |
| 21/2 | Extra Strong | 0.280 | 2.875 | 1,479 | 10 | 1,000 | Gage limited to 1 000 psi |
| 3 | Regular | 0.095 | 3.500 | 388 | 3 | 388 | Full calculated pressure |
| 3 | Extra Strong | 0.304 | 3.500 | 1,307 | 9 | 1,000 | Gage limited to 1 000 psi |
| 31/2 | Regular | 0.095 | 4.000 | 339 | 2 | 339 | Full calculated pressure |
| 31/2 | Extra Strong | 0.321 | 4.000 | 1,201 | 8 | 1,000 | Gage limited to 1 000 psi |
| 4 | Regular | 0.109 | 4.500 | 346 | 2 | 346 | Full calculated pressure |
| 4 | Extra Strong | 0.341 | 4.500 | 1,129 | 8 | 1,000 | Gage limited to 1 000 psi |
| 5 | Regular | 0.125 | 5.552 | 321 | 2 | 321 | Full calculated pressure |
| 5 | Extra Strong | 0.375 | 5.552 | 1,000 | 7 | 1,000 | Exactly 1 000 psi |
| 6 | Regular | 0.134 | 6.625 | 288 | 2 | 288 | Full calculated pressure |
| 6 | Extra Strong | 0.437 | 6.625 | 975 | 7 | 975 | Full calculated pressure |
Related reading: copper nickel pipe hydrostatic test pressure, nickel alloy fittings and flanges overview and asme b16 5 and b16 47 flange size boundary.
Compare the supplier pages for this alloy family, each with dimensions, certification and RFQ information: