Zirconium R60702 R60704 R60705 Pipe | ASME SB-658

Category:
Your Trusted Nickel Alloy Partner
  • Full range pipes plates bars and fittings
  • Certified nickel alloys with strict quality control
  • Strong supply chain with stable factory partnerships
  • Global export experience with fast reliable delivery
  • Professional technical support for demanding applications

The most common specification mistake we see on zirconium enquiries is
ordering UNS R60705 where UNS R60702 was intended. R60705 is not a stronger
or better grade of zirconium: it is a niobium-bearing alloy, and its
chemistry, strength and corrosion behaviour differ enough that the two are
not interchangeable. Getting the grade right at the enquiry stage avoids a
lot of rework later.

ASME SB-658 covers three grades of seamless and welded zirconium pipe:
R60702, R60704 and R60705. The differences between them are worth setting out
before anything else is discussed.

Round zirconium UNS R60702 seamless pipe to ASME SB-658 stacked in the Tailan Metal workshop

Grade comparison to ASME SB-658 Table 1 and Table 3

Element, wt pctR60702R60704R60705
Zirconium + hafnium, min99.297.595.5
Hafnium, max4.54.54.5
Iron + chromium0.2 max0.2 to 0.40.2 max
Tin–1.0 to 2.0–
Niobium––2.0 to 3.0
Oxygen, max0.160.180.18
Hydrogen, max0.0050.0050.005
Nitrogen, max0.0250.0250.025
Carbon, max0.050.050.05
Tensile strength, min, ksi [MPa]55 [380]60 [415]80 [550]
Yield strength, min, ksi [MPa]30 [205]––

R60702 is the commercially pure grade and carries the strongest corrosion
resistance against hydrochloric and sulphuric acid. R60704 introduces 1 to
2 percent tin, which improves strength and is used where higher mechanical duty
is needed. R60705 introduces 2 to 3 percent niobium and reaches 80 ksi
[550 MPa] tensile, giving it the highest strength of the three with corrosion
resistance still ahead of most nickel alloys.

Large diameter zirconium UNS R60705 seamless pipe to ASME SB-658

Where zirconium pipe is used

  • Hydrochloric acid absorption and stripping columns in hydrochloric acid
    production
  • Sulphuric acid dilution and heat exchanger circuits
  • Acetic acid and formic acid handling in the absence of oxidising
    contaminants
  • Fine chemical and pharmaceutical intermediate transfer
  • Pickling and etching lines in the steel and nickel industries

Rectangular and square zirconium UNS R60704 seamless tube to ASME SB-658

Zirconium is not a general corrosion resistant alloy. It has no useful
resistance to wet chlorine at elevated temperature, to oxidising acids
above about 65 degrees Celsius, or to alkalis at any concentration. If any
of those are present in the service, the material selection has to be
revisited rather than the grade adjusted.

Material specification and product range

Product formSpecificationGrades
Seamless and welded pipeASME SB-658 / ASTM B658R60702, R60704, R60705
Butt weld fittingsASME SB-653 / ASTM B653R60702, R60704, R60705
ForgingsASME SB-493 / ASTM B493R60702 and higher grades
TubeASME SB-523 / ASTM B523R60702, R60704, R60705
Bar and wireASME SB-550 / ASTM B550R60702 and higher grades
Strip, sheet and plateASME SB-551 / ASTM B551R60702 and higher grades

Pipe is supplied to the nominal sizes and wall thicknesses of ASME B36.19M
for the S schedules, with outside diameter and wall tolerances to the tables
in SB-658. Thin wall pipe is treated separately for ovality, because thin
wall material develops significant out-of-roundness during final annealing
and straightening.

Certification and inspection

EN 10204 3.1 certification is issued per heat, quoting the grade, the
UNS number and the chemical analysis against SB-658 Table 1. Hydrostatic
testing is available and reported separately. Where the contract calls for
it, the material can be supplied with a specific reversible certificate and
third party inspection can be arranged at the works.

Zirconium is handled as a clean metal throughout. It is not carbon steel
with a coating, and a surface scratch or iron deposit becomes a corrosion
nucleus. We pack zirconium separately from steel and mark every bundle so the
receiving warehouse keeps it apart.

Ordering information

Please give the grade as the UNS number rather than the trade name, the
nominal size and schedule, the length, the quantity, and the certificate
requirement. If the enquiry is for a replacement of an existing line, the
existing material marking is usually sufficient for us to identify the
correct grade. If the service conditions are new to us, include the acid
concentration and temperature so we can confirm suitability before quoting.

Related items include our
zirconium butt weld fittings to ASME SB-653
and zirconium plate, sheet and bar,
which cover the same three grades in other product forms. For the wider
category see nickel alloy pipe and tube,
and the
acid service alloy selection
article covers where zirconium sits against the nickel alloys.

Hydrostatic test pressure for zirconium pipe

Zirconium pipe is proof tested to a rule of its own. ASME SB-658 clause 13.2 requires that each pipe 1/8 in. [3.2 mm] and larger in outside diameter, and with wall thickness of 0.015 in. [0.4 mm] and over, be tested to a hydrostatic pressure sufficient to produce a fiber stress of three fourths of the minimum yield strength of the pipe, provided that the test pressure does not exceed 5000 psi [35 MPa]. The pressure is calculated as P = 2St/D, where S is that three-fourths allowable fiber stress, t is the average wall thickness of the pipe and D is the nominal diameter.

That is a different rule from the one applied to nickel alloy seamless pipe under SB-829, and the difference is not cosmetic. SB-658 fixes the fiber stress as a fraction of the grade’s minimum yield strength rather than deriving an allowable from the material, it uses the average wall rather than the minimum permitted wall, and it caps the result instead of setting a floor.

The minimum yield strengths that feed the calculation are those of SB-658 Table 3: 30 ksi [205 MPa] for R60702, 35 ksi [240 MPa] for R60704 and 55 ksi [380 MPa] for R60705. Applying three fourths of each, the allowable fiber stress works out at 22 500 psi, 26 250 psi and 41 250 psi respectively. The table below gives the resulting maximum test pressure for each grade at each size and schedule, using the nominal wall thicknesses of SB-658 Table X1.1.

These pressures are our own calculation, worked out from the printed formula, the printed yield strengths and the printed nominal wall thicknesses. They are not values printed in the specification, and the actual test pressure on any given order is set by the mill against the pipe it has produced. Where the calculated figure exceeds the 5000 psi [35 MPa] limit of clause 13.2, the specification requires the lower pressure and the table says so.

The practical consequence is worth stating plainly. At the small sizes the calculated pressure runs above the 5000 psi [35 MPa] ceiling of clause 13.2, so the ceiling is what governs and the grade makes no difference to the test: at NPS 1/2 Schedule 40S all three grades are tested to 5 000 psi, because the calculated figures of 5 839, 6 812 and 10 705 psi all exceed it. The point at which the ceiling stops binding differs by grade, since R60705 carries 1.8 times the allowable fiber stress of R60702 (41 250 psi against 22 500 psi). For R60702 the calculated figure first falls below the ceiling at NPS 3/4 Schedule 40S, for R60704 at NPS 1-1/4 Schedule 40S, and for R60705 not until NPS 3-1/2 Schedule 40S. Below those points the grade does matter, because R60705 carries the higher fiber stress and is tested to a correspondingly higher pressure. At NPS 4 Schedule 40S, for example, R60702 is tested to 2 370 psi while R60705 is tested to 4 345 psi, and at NPS 12 Schedule 40S the three grades are tested to 1 324 psi, 1 544 psi and 2 426 psi.

Dimensions and tolerances

SB-658 Table X1.1 is a reprint of Table 1 of ANSI B36.19 with SI units added, and it is the table to order against. Note one point of detail: at NPS 5 the specification prints an outside diameter of 5.583 in. [141.3 mm], while the ANSI B36.19 Table 1 reprints carried in SB-829, SB-775, SB-861 and SA-790 all print 5.563 in. [141.30 mm] for the same size. The two figures cannot both be right, since 5.583 in. converts to 141.8 mm, not 141.3 mm. We order and inspect to the mill’s certified dimension and flag the discrepancy rather than reconcile it ourselves.

Permissible diameter variations are given in SB-658 Table 4 for seamless pipe only: 1/64 in. [0.4 mm] over and 1/32 in. [0.8 mm] under up to NPS 1-1/2, widening to 3/32 in. [2.4 mm] over and 1/32 in. [0.8 mm] under from NPS 8 to NPS 12. Tolerances on welded pipe are as agreed between the manufacturer and the purchaser. Wall thickness variation is limited to 12.5 % of the nominal wall by clause 9.2, and for thin-wall pipe, defined as a wall of 3 % or less of the outside diameter, clause 9.1.2 limits ovality to 1.5 % of the specified outside diameter.

NPSScheduleNominal wall, in. (mm)R60702 max test pressureR60704 max test pressureR60705 max test pressure
1/840S0.0685,000 psi (capped)
34 MPa
5,000 psi (capped)
34 MPa
5,000 psi (capped)
34 MPa
1/880S0.0955,000 psi (capped)
34 MPa
5,000 psi (capped)
34 MPa
5,000 psi (capped)
34 MPa
1/440S0.0885,000 psi (capped)
34 MPa
5,000 psi (capped)
34 MPa
5,000 psi (capped)
34 MPa
1/480S0.1195,000 psi (capped)
34 MPa
5,000 psi (capped)
34 MPa
5,000 psi (capped)
34 MPa
3/840S0.0915,000 psi (capped)
34 MPa
5,000 psi (capped)
34 MPa
5,000 psi (capped)
34 MPa
3/880S0.1265,000 psi (capped)
34 MPa
5,000 psi (capped)
34 MPa
5,000 psi (capped)
34 MPa
1/240S0.1095,000 psi (capped)
34 MPa
5,000 psi (capped)
34 MPa
5,000 psi (capped)
34 MPa
1/280S0.1475,000 psi (capped)
34 MPa
5,000 psi (capped)
34 MPa
5,000 psi (capped)
34 MPa
3/440S0.1134,843 psi
33 MPa
5,000 psi (capped)
34 MPa
5,000 psi (capped)
34 MPa
3/480S0.1545,000 psi (capped)
34 MPa
5,000 psi (capped)
34 MPa
5,000 psi (capped)
34 MPa
140S0.1334,551 psi
31 MPa
5,000 psi (capped)
34 MPa
5,000 psi (capped)
34 MPa
180S0.1795,000 psi (capped)
34 MPa
5,000 psi (capped)
34 MPa
5,000 psi (capped)
34 MPa
11/440S0.1403,795 psi
26 MPa
4,428 psi
31 MPa
5,000 psi (capped)
34 MPa
11/480S0.1915,000 psi (capped)
34 MPa
5,000 psi (capped)
34 MPa
5,000 psi (capped)
34 MPa
11/240S0.1453,434 psi
24 MPa
4,007 psi
28 MPa
5,000 psi (capped)
34 MPa
11/280S0.2004,737 psi
33 MPa
5,000 psi (capped)
34 MPa
5,000 psi (capped)
34 MPa
240S0.1542,918 psi
20 MPa
3,404 psi
23 MPa
5,000 psi (capped)
34 MPa
280S0.2184,131 psi
28 MPa
4,819 psi
33 MPa
5,000 psi (capped)
34 MPa
21/240S0.2033,177 psi
22 MPa
3,707 psi
26 MPa
5,000 psi (capped)
34 MPa
21/280S0.2764,320 psi
30 MPa
5,000 psi (capped)
34 MPa
5,000 psi (capped)
34 MPa
340S0.2162,777 psi
19 MPa
3,240 psi
22 MPa
5,000 psi (capped)
34 MPa
380S0.3003,857 psi
27 MPa
4,500 psi
31 MPa
5,000 psi (capped)
34 MPa
31/240S0.2262,542 psi
18 MPa
2,966 psi
20 MPa
4,661 psi
32 MPa
31/280S0.3183,578 psi
25 MPa
4,174 psi
29 MPa
5,000 psi (capped)
34 MPa
440S0.2372,370 psi
16 MPa
2,765 psi
19 MPa
4,345 psi
30 MPa
480S0.3373,370 psi
23 MPa
3,932 psi
27 MPa
5,000 psi (capped)
34 MPa
540S0.2582,080 psi
14 MPa
2,426 psi
17 MPa
3,812 psi
26 MPa
580S0.3753,023 psi
21 MPa
3,526 psi
24 MPa
5,000 psi (capped)
34 MPa
640S0.2801,902 psi
13 MPa
2,219 psi
15 MPa
3,487 psi
24 MPa
680S0.4322,934 psi
20 MPa
3,423 psi
24 MPa
5,000 psi (capped)
34 MPa
840S0.3221,680 psi
12 MPa
1,960 psi
14 MPa
3,080 psi
21 MPa
880S0.5002,609 psi
18 MPa
3,043 psi
21 MPa
4,783 psi
33 MPa
1040S0.3651,528 psi
11 MPa
1,783 psi
12 MPa
2,801 psi
19 MPa
1080S0.5002,093 psi
14 MPa
2,442 psi
17 MPa
3,837 psi
26 MPa
1240S0.3751,324 psi
9 MPa
1,544 psi
11 MPa
2,426 psi
17 MPa
1280S0.5001,765 psi
12 MPa
2,059 psi
14 MPa
3,235 psi
22 MPa

Related reading: zirconium pipe schedule and wall thickness table, zirconium forging fittings in SB-653 and nickel alloy pipe and tube product range.

Product Enquiry