ASME SB-637 is the specification that ties a bar order to a named heat-treatment condition. An order written against it states the alloy, the product form and the condition, leaving the mill no latitude to substitute a different solution treatment or an abbreviated ageing cycle. The grades buyers know by name — Inconel X-750, Nimonic 80A, Waspaloy — are precipitation-hardening alloys whose useful strength exists only after ageing. Our cold drawn bars and forged bars listings cover the wider range; this page covers what SB-637 controls.
| ASME specification | Grade | UNS | Product form | Delivery condition |
|---|---|---|---|---|
| SB-637 | Inconel X-750 | N07750 | Rod, bar, forgings, forging stock | Type 1, 2 or 3 aged |
| SB-637 | Nimonic 80A | N07080 | Rod, bar, forging stock | Solution, stabilised, aged |
| SB-637 | Waspaloy | N07752 | Rod, bar, forging stock | Type 1 or 2 aged |
| SB-637 | Alloy 263 | N09925 | Rod and bar | Solution, aged |
| SB-637 | Inconel 725 | N07725 | Rod and bar | Solution, aged |
Diameter and length tolerances are set by SB-637 Table 5 for cold-worked rod and bar and Table 6 for hot-worked rod and bar. Cut lengths carry a permissible variation of + 1/8 in. (3.17 mm), −0.
Composition limits below are from SB-637 Table 1. The strengthening additions separate the alloys: X-750 and Waspaloy carry niobium plus tantalum between 0.70 and 1.20 %, while Nimonic 80A reaches its strength from aluminium and titanium alone.
| Element | X-750 N07750 | Nimonic 80A N07080 | Waspaloy N07752 |
|---|---|---|---|
| Chromium | 14.00–17.00 % | 18.00–21.00 % | 14.50–17.00 % |
| Nickel | 70.00 % min | remainder | 70.0 % min |
| Nb + tantalum | 0.70–1.20 % | — | 0.70–1.20 % |
| Titanium | 2.25–2.75 % | 1.80–2.70 % | 2.25–2.75 % |
| Aluminium | 0.40–1.00 % | 0.50–1.80 % | 0.40–1.00 % |
| Iron | 5.00–9.00 % | 3.00 % max | 5.00–9.00 % |
SB-637 Table 2 sets the recommended treatment and Table 3 the room-temperature limits that apply afterwards. The supplier must demonstrate that the material meets these fully heat-treated properties.
| Condition | Tensile min | Yield min | Elongation min | Hardness |
|---|---|---|---|---|
| X-750 Type 1 | 140 000 psi (965 MPa) | 90 000 psi (620 MPa) | 8 % | 262 min (26 Rc min) |
| X-750 Type 2 | 170 000 psi (1170 MPa) | 115 000 psi (790 MPa) | 18 % | 302 to 363 (32–40 Rc) |
| Nimonic 80A | 135 000 psi (930 MPa) | 90 000 psi (620 MPa) | 20 % | — |
| Waspaloy Type 1 | 160 000 psi (1103 MPa) min, 185 000 psi (1276 MPa) max | 100 000 psi (689 MPa) min, 130 000 psi (896 MPa) max | 20 % | 267 to 363 (27–40 Rc) |
X-750 Type 1 is solution annealed at 2100 °F (1149 °C), stabilised at 1550 °F (843 °C) and aged at 1300 °F (704 °C); Type 2 uses an 1800 °F (982 °C) solution with ageing at 1350 °F (732 °C). Nimonic 80A is solution treated at 1950 °F (1066 °C), stabilised at 1560 °F (849 °C) and aged at 1290 °F (699 °C). Stress-rupture data in Table 4 sizes the bolt: X-750 Type 1 is rated at 1350 °F (732 °C) and 45 000 psi (310 MPa) for a minimum of 100 hours, Nimonic 80A at 1400 °F (760 °C) and 47 000 psi (325 MPa) for 23 hours.
Gas turbine fasteners, bolting for high-temperature flanged joints, disc and hub hardware, spring wire and valve stems, exhaust bellows, nuclear reactor internals, and bolting stock for energy and chemical plant. We also supply the matching Inconel 718 bolt stock.
Material is supplied with certification stating that it was manufactured, sampled, tested and inspected in accordance with SB-637. Chemical analysis is one test per lot; tension, hardness and stress-rupture are one test per lot. Third-party inspection and full heat traceability can be arranged.
Send the alloy designation and UNS number, the heat-treatment type, the diameter or distance between parallel surfaces, the length, and the delivery condition — solution annealed, solution plus stabilisation, or fully heat treated. Our hot rolled round bar and nickel alloy round bars pages carry the dimensional options, and how heat treatment dictates metal performance explains the effect of each ageing cycle. If you are still comparing designations, our nickel alloy grade cross reference by UNS and trade name guide lists every precipitation-hardening grade we stock.