A practical comparison of 254SMO (S31254), 904L (N08904) and AL-6XN (N08367) for seawater and chloride service: PREN, standards, strength and where each grade pays off.
When chloride concentration, temperature or crevice conditions push ordinary 316L past its limits, three grades come up in almost every enquiry: 254SMO (UNS S31254), 904L (UNS N08904) and AL-6XN (UNS N08367). They are not interchangeable. This guide compares them on the properties that actually decide a piping or equipment specification.
All three are high-molybdenum austenitic grades, but they sit at different points on the pitting-resistance scale. PREN (pitting resistance equivalent number) is a useful first filter, not a substitute for testing at your actual temperature and pH.
| Grade | UNS | Cr (%) | Mo (%) | N (%) | Typical PREN |
|---|---|---|---|---|---|
| 254SMO | S31254 | 19.5-20.5 | 6.0-6.5 | 0.18-0.22 | ~43 |
| AL-6XN | N08367 | 20.0-22.0 | 6.0-7.0 | 0.18-0.25 | ~43-46 |
| 904L | N08904 | 19.0-23.0 | 4.0-5.0 | ≤0.10 | ~34-36 |
Read the PREN column as a ranking, not an absolute: AL-6XN and 254SMO are the high-molybdenum tier, while 904L is a lower-molybdenum, high-nickel grade aimed more at reducing-acid service than at severe seawater pitting.
The form you order determines the specification, and the three grades do not share identical coverage:
Source each form to the correct book of specifications. Mixing an A403 fitting with a B677 pipe without confirming pressure-temperature ratings is a common procurement error.
The workhorse for seawater cooling, desalination brine, bleach plants and pulp mill chlorine dioxide service. Its combination of about 6% molybdenum and nitrogen gives strong resistance to pitting and crevice corrosion at a cost below many nickel-base alternatives. Start with our 254SMO seamless pipe to ASTM A312 and 254SMO butt-weld fittings.
Chosen where higher strength and slightly higher molybdenum help, notably large-diameter seawater piping, reverse osmosis and flue-gas desulfurisation scrubbers. It is often the economical upgrade from 254SMO when wall thickness can be reduced. See AL-6XN seamless pipe to ASTM B690 and AL-6XN plate to ASTM B688.
High nickel and copper, moderate molybdenum. It shines in sulfuric, phosphoric and other reducing acid services rather than stagnant seawater. If your medium is acid, not chloride, 904L is frequently the better value. Compare 904L seamless pipe to ASTM B677.
No. 254SMO (S31254) has about 6% molybdenum and nitrogen for a PREN near 43, while 904L (N08904) has about 4-5% molybdenum and little nitrogen, giving roughly 34-36. 254SMO is the stronger choice for chloride pitting; 904L is favoured for reducing acids.
Often, but not automatically. Their corrosion resistance is comparable and AL-6XN is somewhat stronger, which can allow thinner walls. Check the governing code, pressure rating and fabrication qualification before substituting.
Prices move with nickel and molybdenum markets, so no fixed ranking holds. AL-6XN and 254SMO are broadly comparable; 904L is usually lower-cost but may not meet a chloride-service requirement. Request a current quote against your exact specification.
Tailan Metal supplies all three grades as pipe, fittings, flanges and plate with mill certificates. Send your specification for a quotation and our team will confirm grade, standard and certification.