When a buyer asks us to compare MC Alloy with the nickel-chromium-molybdenum grades they already run, the honest answer is that MC Alloy is not a corrosion-first alloy. It is a corrosion-and-heat alloy, and it wins on chemistry only in a narrow band of duties.
Every item is produced under a material specification that makes certification and a test report mandatory, and dimensions follow the dimensional standards referenced in that specification.
| Grade | UNS | Cr | Mo | Ni | Fe max | Ti | C max | Tensile / Yield |
|---|---|---|---|---|---|---|---|---|
| MC Alloy | N06044 | 43.5-45.3 | 0.80-1.20 | Bal. | 0.3 | 0.10-0.30 | 0.02 | 100 / 45 ksi |
| Alloy 35 | N06035 | 32.25-34.25 | 7.60-9.00 | rem. | 2.0 | – | 0.050 | 85 / 35 ksi |
| C-4 | N06455 | 14.0-18.0 | 14.0-17.0 | rem. | 3.0 | 0.7 max | 0.015 | 100 / 40 ksi |
| C-22 | N06022 | 20.0-22.5 | 12.5-14.5 | rem. | 2.0-6.0 | – | 0.015 | 100 / 45 ksi |
| 686 | N06686 | 19.0-23.0 | 15.0-17.0 | rem. | 5.0 | 0.02-0.25 | 0.010 | 100 / 45 ksi |
Composition limits are taken from the chemical requirement table of the governing ASME specification. Compare the molybdenum and chromium columns before quoting a substitution.
| Product form | ASME specification | UNS grade | Condition | Key note |
|---|---|---|---|---|
| Round bar | SB-574 | N06044 | Hot or cold finished, solution annealed | 5/16 to 3-1/2 in. diameter |
| Rod | SB-574 | N06044 | Hot or cold finished, annealed | 2 to 12 ft random mill lengths |
| Plate and sheet | SB-575 | N06044 | Annealed and descaled | Same chemistry family |
| Forgings | SB-564 | N06044 | Solution annealed | B564 per SB-366 Table 2 |
| Pipe | SB-622 | N06044 | Solution annealed | B622 per SB-366 Table 2 |
Heat treatment. 2100-2230 °F [1150-1220 °C], rapid air or water quench, per ASME SB-366 Table 3 (CR MC / WPHMC grade).
Mechanical properties. Tensile 100 000 psi (690 MPa) min, yield 45 000 psi (310 MPa) min, elongation 30% min (SB-574 Table 5).
Nitric-hydrofluoric acid service, high temperature oxidation and sulfidation resistant components, heat treating fixtures and furnace internals, and chemical processing equipment where a high chromium, low molybdenum composition is required. It is not a substitute for the C-family grades in table above: those carry far more molybdenum.
Chemical analysis to ASTM E1473, tensile testing to ASTM E8/E8M, hardness to ASTM E140, macro-etch for forging stock, and EN 10204 3.1 certification with heat number traceability.
Provide the diameter, length and delivery condition you need, together with the service temperature and medium, and we will confirm availability, tolerance class and the certification documentation.
For the same alloy in a different shape, see nickel-chromium-molybdenum-tungsten round bar to ASME SB-446 and cold drawn nickel alloy round bars. The wider range is under nickel alloy round bars.
For background on the numbers above, see nickel alloy material selection and properties.
For service-specific selection read how heat treatment governs round bar performance.